< img height="1" width="1" style="display:none" src="https://www.facebook.com/tr?id=28308886678697114&ev=PageView&noscript=1" />

Produce precision parts that exceed industry standards.

Provide efficient production and faster design to delivery.

Manufacture prototypes and products that meet medical safety standards at competitive prices.

Improve efficiency with precise, fast, and constant part quality.

Create and test products quickly to bring them to market.

Deliver machinery that beats the competition.

Empower to innovate faster,maximizing performance.

Speed up innovation and development.

Bring new, affordable products to market faster.

Produce precision parts that exceed industry standards.

Provide efficient production and faster design to delivery.

Manufacture prototypes and products that meet medical safety standards at competitive prices.

Improve efficiency with precise, fast, and constant part quality.

Create and test products quickly to bring them to market.

Deliver machinery that beats the competition.

Empower to innovate faster,maximizing performance.

Speed up innovation and development.

Bring new, affordable products to market faster.

Steel Machining Services

Customize steel CNC machining services for customers at competitive prices, from prototyping to manufacturing, and get excellent surface finish, high precision, corrosion-resistant CNC machined steel parts in a short time.

Custom Steel Machining Service

Our Steel Machining Capabilities

Steel is an important iron-carbon alloy with carbon content ranging from 0.02% to 2.11%. It combines the high strength of iron with the hardness and wear resistance of carbon while having excellent ductility and forgeability. It is the most widely used material in CNC machining with high tensile strength, high yield point, good impact toughness, and excellent fatigue strength. CNC machining steel is widely used in aerospace, construction, machinery, chemical industry, power, and other industries. In addition, the recyclability of steel also reflects its environmental protection and sustainable characteristics.

Price

$$$

Lead Time<10 days
Wall Thickness0.75 mm
Tolerances

±0.005″ (±0.125mm)

Max Part Size

200 cm x 80 cm x 100 cm

Available Steel at NOBLE

Carbon Steel: 1018, 1020, 1025, 1045, 1215, 4130, 4140, 4340, 5140, A36, ST37 
Alloy Steel: 4J36 
Die Steel: 718H, P20, S136, S7 
Chisel Tool Steel: D2/SKD11, SKD61 
High Speed Steel: SKH51 Spring Steel: 1566, 9260 Tool Steel: A2 Bearing Steel: E51100/SUJ1, E52100/SUJ2 
Galvanized Steel: SGCC / SECC SPCC

Our Steel-Machining-Capabilities

Characteristics of Steel Machining Materials

Steel parts machining and manufacturing is one of our main type,below is some common information about Steel.

FeaturesInfo
SubtypesQ195, Q215, Q235, Q255, Q275, 08 and 08F Steel, 10 an, 10F Steel, 20 Steel, 45 Steel, 40Cr Steel, 35CrMo Steel, 42CrMo Steel
ProcessCNC machining, sheet metal fabrication,die casting
ToleranceWith drawing: as low as +/- 0.005 mm No drawing: ISO 2768 medium
ApplicationsFixtures and mounting plates; draft shafts, axles, torsion bars
Finishing OptionsBlack Oxide, ENP, Electropolishing, Media Blasting, Nickel Plating, Powder Coating, Tumble Polishing, Zinc Plating

 

Pros and Cons of Steel for CNC Machining

Aluminum is well suited for CNC machining due to its light weight, machinability, and versatility, making it suitable for a wide range of industries and favored by CNC machining manufacturers, however, it faces some challenges, such as lower strength compared to steel, susceptibility to wear, and potential issues related to thermal expansion and corrosion. Choosing the right aluminum machining method can mitigate these disadvantages for most applications.

Pros-of-steel-for-CNC-Machining
Cons-of-steel-for-CNC-Machining

Types of Steel Machining Materials

Steel has a wide range of mechanical properties, and the choice of these steels depends on the specific requirements of the CNC machining process and the application’s need for strength, durability, and wear or corrosion resistance. Each steel type offers unique advantages for specific applications in industries ranging from manufacturing to automotive and aerospace. Here are some of the key properties of common steel alloys used in CNC machining.

Carbon Steel Q195

Carbon Steel Q195

With low carbon content, it offers good plasticity, toughness, machinability, and weldability but moderate strength. Commonly used for rolling thin sheets and coils, as well as cold- and hot-rolled galvanized and tinplate composite sheets for roofing panels, decorative sheets, general-purpose dust removal piping, packaging containers, etc.

Yield Strength(MPa): 195MPa

Elongation at Break(%): ≥33% (for thicknesses ≤16mm) ≥32%(for thicknesses>16-40mm)

Hardness(Brinell): 130-240HB

Density(G/m³): ≈7.85 G/m³

Maximum Temp: -20~500℃ at usually (Varies with heat treatment)

Carbon Steel Q215

Carbon Steel Q215

Slightly stronger than Q195, it shares similar applications and is also extensively used for welded steel pipes, galvanized welded pipes, furnace supports, anchor bolts, bolts, round nails, wood screws, stamped iron hinges, and other hardware components.

Yield Strength(MPa): 215MPa (decreasing with increasing thickness)

Elongation at Break(%): ≥31% (for thicknesses ≤40mm)

Hardness(Brinell): 230HB

Density(G/m³): ≈7.85 G/m³

Maximum Temp: -40~200℃ at usually

Carbon Steel Q235

Carbon Steel Q235

Balances strength, plasticity, and weldability well. It is the most widely used grade. Applications include rolled steel shapes (such as round bars, square bars, flat bars, angle bars, I-beams, channel beams, window frame steel, etc.) and medium-thick steel plates for construction and engineering structures (like reinforcing steel bars, factory building frames, high-voltage transmission towers, bridges, vehicles, boilers, containers, ships, etc.). It is also widely used for mechanical parts with moderate performance requirements.

Yield Strength(MPa): 235MPa

Elongation at Break(%): 26%

Hardness(Brinell): 170-210HB

Density(G/m³): ≈7.85 G/m³

Maximum Temp: 0~350℃ at usually

Carbon Steel Q255

Carbon Steel Q255

Similar properties to Q235 but with slightly higher strength and lower plasticity. Less commonly used than Q235, primarily for riveted and bolted structures.

Yield Strength(MPa): 255MPa

Elongation at Break(%): 24% (for thicknesses ≤16mm)

Hardness(Brinell): HB220~250

Density(G/m³): ≈7.85 G/m³

Maximum Temp: -20~50℃ at usually

Carbon Steel Q275

Carbon Steel Q275

Higher strength and hardness with good wear resistance. Used for manufacturing shafts, agricultural implements, wear-resistant parts, rail joint splints, base plates, wheels, rolls, etc.

Yield Strength(MPa): 275MPa

Elongation at Break(%): 17~22%

Hardness(Brinell): 270~400HB

Density(G/m³): ≈7.85 G/m³

Maximum Temp: 200~300℃ at usually

Carbon Steel 08F

Carbon Steel 08F

Used for rolling thin sheets, deep-drawn products, oil drums, high-quality enamelware, and also for pipes, gaskets, and parts requiring low core strength such as carbonized and cyanided parts, welding electrodes, etc.

Yield Strength(MPa): 175MPa

Elongation at Break(%): ≥35%

Hardness(Brinell): 131HB

Density(G/m³): ≈7.85 G/m³

Maximum Temp: ≥200℃ at usually

Carbon 10 and 10F Steel

Carbon Steel 10F

Suitable for cold deep-drawing products under 4mm thick, such as deep-drawn containers and artillery shells. Also used for boiler tubes, oil drum covers, steel strips, steel wires, welded parts, and mechanical parts.

Yield Strength(MPa): 185MPa

Elongation at Break(%): ≥30%

Hardness(Brinell): 137HB

Density(G/m³): ≈7.85 G/m³

Maximum Temp: ≥470℃ at usually

Carbon 20 Steel

Carbon 20 Steel

Good weldability and plasticity, suitable for cold pressing and cold rolling. Often used for manufacturing parts and components like bolts, nuts, bearings, and pins.

Yield Strength(MPa): 355MPa

Elongation at Break(%): ≥25%

Hardness(Brinell): 156HB

Density(G/m³): ≈7.85 G/m³

Maximum Temp: -20~425℃ at usually

Carbon-45-Steel

Carbon 45 Steel

Excellent mechanical properties and heat treatment capabilities. Commonly used for manufacturing mechanical parts and components such as gears, racks, chains, and pins.

Yield Strength(MPa): 355MPa

Elongation at Break(%): ≥16%

Hardness(Brinell): 197HB

Density(G/m³): ≈7.85 G/m³

Maximum Temp: -20~400℃ at usually

Carbon 40Cr Steel

Carbon 40Cr Steel

High strength and wear resistance. Often used for manufacturing high-strength, high-hardness mechanical parts such as machine tool shafts, wheel shafts, transmission gears, and racks.

Yield Strength(MPa): 785MPa

Elongation at Break(%): ≥9%

Hardness(Brinell): 207HB

Density(G/m³): ≈7.85 G/m³

Maximum Temp: ≤200℃ at usually

Carbon 35CrMo Steel

Carbon 35CrMo Steel

Good high-temperature resistance and high strength. Suitable for heavy-duty parts under high temperature and pressure, such as forging dies, automotive transmission shafts, and hydraulic cylinders.

Yield Strength(MPa): 835MPa

Elongation at Break(%):≥12 %

Hardness(Brinell): 229 (annealed or high-temperature tempered)

Density(G/m³): ≈7.85 G/m³

Maximum Temp: 500°C at usually

Carbon 42CrMo Steel

Carbon 42CrMo Steel

High strength and toughness. Used for manufacturing critical parts of large machinery, such as wind turbine bearings and aerospace engine components.

Yield Strength(MPa): 930~1100MPa at usually

Elongation at Break(%): ≥12%

Hardness(Brinell): 147~298HBW

Density(G/m³): ≈7.85 G/m³

Maximum Temp: 530°C at usually

Surface Finishing Options for Steel Machining

NOBLE has more than ten years of experience in surface treatments that can improve the performance and aesthetics of CNC-machined steel parts. Each surface treatment is tailored to meet the unique needs of your steel parts, ensuring they are suitable for any scenario.

Electroplating

Electroplating

Electroplating uses electrolytic principles to deposit a layer of metal or alloy coating on the metal surface. During electroplating, the workpiece serves as the cathode, and metal ions in the plating solution receive electrons at the cathode, reducing to metal atoms and depositing to form a coating. Electroplated coatings exhibit excellent electrical conductivity, corrosion resistance, hardness, and aesthetics.

As Machined

As machined 

The as-machined finish highlights precision machining marks, offering a natural, sleek look. Ideal for functional parts, it’s cost-effective, maintaining tight tolerances without extra machining.

Passivation 1

Passivation

To increase surface hardness and dissipate heat, we use anodizing techniques to enhance the look of parts and blend well for painting and priming.

powder coating

Powder Coating

Powder coating applies a heat-cured, durable finish, resistant to chipping, scratching, and fading. It offers aesthetic flexibility with various colors, perfect for outdoor equipment, automotive parts, and durable consumer products.

Shot-Peening

Shot Peening

Shot peening involves projecting abrasive particles at high speed onto the surface of a workpiece to remove surface contaminants, oxide layers, and old coatings, while increasing surface roughness to enhance adhesion for subsequent treatments (e.g. painting, electroplating). 

Bluing--Blackening

Bluing / Blackening

Bluing and blackening rapidly oxidize the surface of steel products, forming a dense oxide film to enhance corrosion resistance. During bluing and blackening, steel products are heated in an oxidizing medium, causing surface oxidation reactions to produce a blue-black or black oxide film. This film offers good corrosion resistance, suitable for rust prevention of steel products.

Physical-Vapor-Deposition-(PVD)

Physical Vapor Deposition (PVD)

PVD deposits material atoms or molecules onto the substrate surface in a vacuum through physical methods (e.g. evaporation, sputtering). PVD coatings exhibit high hardness, low friction coefficients, and high temperature resistance. PVD technologies include vacuum evaporation coating, sputtering coating, and ion plating.

Pickling

Pickling

Pickling employs acid solutions (such as sulfuric acid, hydrochloric acid, nitric acid, etc.) to remove oxide scales, rust, and oil from metal surfaces. During pickling, chemical reactions between the acid solution and metal surface contaminants generate soluble salts or gases, achieving surface cleanliness. Pickling is widely used in surface treatment of steel, non-ferrous metals, and other metallic materials.

Phosphating

Phosphating

Phosphating forms an insoluble phosphate coating on the metal surface to enhance corrosion resistance and coating adhesion. In the phosphating process, a chemical reaction between the metal surface and a phosphate solution produces a dense phosphate coating. This coating exhibits excellent corrosion resistance, adhesion, lubrication.

Chemical Plating

Chemical Plating

Chemical plating deposits a layer of metal or alloy coating on the metal surface without applying an external current, through chemical reduction reactions. Chemical plating offers uniform coatings with strong adhesion, simplicity in process, and is suitable for complex shapes and blind-hole parts.

Chemical-Vapor-Deposition-(CVD)

Chemical Vapor Deposition (CVD)

CVD forms a solid coating on the substrate surface through gas-phase chemical reactions. CVD coatings possess exceptional chemical stability, high temperature resistance, and mechanical properties, suitable for manufacturing hard coatings, high-temperature, and corrosion-resistant components.

Ion Implantation

Ion Implantation

Ion implantation injects high-energy ion beams into the metal surface, altering the composition and structure of the surface layer through collisions and energy exchange between ions and substrate atoms, thereby improving its properties. Ion implantation offers advantages such as high processing temperatures, short processing times, and controllable implanted elements, suitable for modifying hardness, wear resistance, and corrosion resistance of metal surfaces.

Laser-Surface-Treatment

Laser Surface Treatment

Laser surface treatment rapidly heats and cools localized areas of the metal surface using high-energy-density laser beams, achieving surface quenching, cladding, alloying, etc. Laser surface treatment offers advantages such as fast processing speeds, high precision, and small heat-affected zones, significantly enhancing the hardness, wear resistance, and fatigue strength of metal surfaces.

Custom Steel Machining Parts Display

Check out our over ten years of custom steel machining, including precision steel prototypes and parts from our valued customers.

Applications of Steel CNC Machining

Steel is one of the most widely used materials in CNC machining, with applications spanning a wide range of industries. Steel’s versatility, strength, and variety make it an ideal choice for producing precision parts for a variety of industries. Here’s a closer look at industry-specific applications for steel in CNC machining:

Automotive

Automotive Industry

Steel is widely used in the automotive industry for its strength, durability, and cost-effectiveness. CNC machining can produce high-precision CNC machined steel parts that are critical to vehicle performance and safety. In the transmission components of automobiles, gears, shafts, and bearings made of steel are precisely machined to achieve a smooth and reliable transmission system.

Aerospace

Aerospace Industry

Steel is a key material in the aerospace industry because it can withstand extreme temperatures and high stresses. Aerospace components require materials that provide both strength and weight reduction. It is often used in aircraft, because fuselage components, landing gear components and fuselage structures are usually made of alloy steel and maraging steel because of their high strength-to-weight ratio and fatigue durability, while parts exposed to high temperatures, such as turbine blades and engine casings, are made of high-performance alloy steel and stainless steel.

Medical Devices

Medical Industry

Steel is widely used in the medical industry for its biocompatibility, corrosion resistance, and ability to be CNC machined into precise, high-quality components. Widely used in surgical instruments, it is used to manufacture surgical tools such as scalpels, forceps, and scissors. The material must be highly resistant to corrosion and withstand the sterilization process. Stainless steel and titanium alloys are used to manufacture medical implants such as joint replacements, dental implants, and bone screws. CNC machining steel ensures precise shapes and tolerances for a proper fit.

Tool and Die Industry

Tool and Die Industry

Tool steel and high-speed steel are essential materials for making molds and cutting tools, as these materials require high hardness, wear resistance, and the ability to withstand extreme conditions. Mainly used in injection molds, tool steel is often used to make injection molds to produce high-precision plastic parts; and die-casting molds, steel is used to make molds for metal parts in the automotive and consumer goods industries; it can also be used as cutting tools, ensuring that high-speed steel and carbide tools are used in CNC machining operations to cut, drill and mill other materials with high precision.

Oil & Gas

Oil & Gas Industry

Steel is indispensable in the oil and gas industry due to its high strength, corrosion resistance, high pressure and high temperature resistance. It is widely used in wind turbine structural frames and components such as shafts, gears and bearings. Steel is also essential in the nuclear power industry for the manufacture of reactor pressure vessels, steam generators and piping systems because of their ability to withstand radiation and high temperatures. In addition, steel can be used to manufacture drill bits, pumps, valves and other drilling equipment for the extraction of oil, natural gas, etc. due to its high strength.

Industrial-Equipment2

Industrial Equipment

Steel’s strength, durability, and flexibility make it a mainstay of the heavy machinery industry. CNC machining steel ensures that components are manufactured to precise dimensions for heavy-duty applications. Beams, columns, and frame members made from steel are fundamental to building construction. Steel’s strength allows it to be formed into large, stable structures, while CNC machining allows for precise cutting and assembly. Steel is used to manufacture large machinery such as cranes, bulldozers, and excavators, which require components such as gears, shafts, and hydraulic systems that can withstand heavy loads and harsh operating conditions.

If you are looking for a rapid prototyping manufacturer or a CNC machine shop to fabricate small, medium-volume, or mass-production products, NOBLE is an ideal choice. Our well-trained and experienced staff manufactures parts in line with drawings on modern CNC machines, with the highest accuracy and processing quality in all sizes.In addition, we provide professional design considerations for your CNC machining projects.

Want to get the most professional and fastest service for your CNC machining project? Upload your CAD files now and obtain a quote!

Scroll to Top

Leave A Message!

Contact Form Demo (#3)

Please attach your 3D drawing. We respect your intellectual property rights and support signing a non-disclosure agreement. Or send your RFQ via email. IM@nobleai.cn

If you have any questions, please do not hesitate to contatct with us.
Customer Cooperation Cases